Surface analysis and cell biology technique in understanding degradation of natural temporary teeth collected from area with high pollution.

Domenii publicaţii > Chimie + Tipuri publicaţii > Articol în revistã ştiinţificã

Autori: Demetrescu I., Iordachescu D., D. Ionita, S. Manea ,

Editorial: Key Engineering Materials (Proceedings Bioceramics 21), 396-398, p.35-38, 2009.

Rezumat:

The aim of this paper is to correlate surface features of degraded temporary teeth from area with high pollution with the cell culture,adhesion and proliferation of human gingival fibroblasts (HGF).

Cuvinte cheie: analiza de suprafata, tehnici de biologie celulara, dinti temporari // Surface analysis,, cell biology technique, temporary teeth