Shell Buckling of Carbon Nanotubes Using Nanoindentation

Domenii publicaţii > Stiinte ingineresti + Tipuri publicaţii > Articol în revistã ştiinţificã

Autori: L. Munteanu and V. Chiroiu

Editorial: Tech Science Press, Computer Modeling in Engineering & Sciences, 48(1), p.27-41, 2009.

Rezumat:

The long-range nanoindentation response of carbon nanotubes is studied
using a new method that combines the features of Nonlocal Theory and Molecular
Mechanics. The deformation of compressed multiple walled carbon nanotubes
is investigated, with the emphasis on the simulation of the nanoindentation technique
in order to compare the present method to available experimental results

Cuvinte cheie: Carbon nanotubes; Molecular mechanics; Nonlocal theory; Buckling; Nanoindentation.

URL: http://www.techscience.com/doi/10.3970/cmes.2009.048.027.pdf